Our China project: understand the basic situation of the site and the measurement site

July 13, 2021

Latest company news about Our China project: understand the basic situation of the site and the measurement site

 

Process:

The cast polyurethane resin is prepared by mixing two components, one a liquid polyol and the other an isocyanate in correct proportions, add SBR granules and then blend at site to form a viscous liquid compound. Then spread on to the base of the track by paving machine, to the full thickness required. The liquid resin mix is then given a textured finish by broadcasting specially formulated colored EPDM rubber granules on the surface and allowing the polyurethane to cure. Following cure, the excess surfacing granules are removed. Finally go with the line marking.